X5CrNi17-7 - Material

X5CrNi17-7 belongs to group Stainless steels (EN)

Applus+ Materials Portal

X5CrNi17-7 is part of Applus+ Materials Portal, it belongs to Steel, Stainless steels, Stainless steels (EN), it is specified in DIN EN 10088-1 : 2005-09. Among others, values can be offered for Yield Strength (1.0% offset) [MPa], Yield Strength (0.2% offset) [MPa], Nominal Size [mm], Elongation A80 [%], Tensile Strength [MPa], Elongation A [%], Hardness HB | HBW in a range of (20;550)°C and for Thermal Conductivity [W/m*K], Young's Modulus [GPa], Mean Specific Heat Capacity [kJ/(kg*K)], Density [g/cm³], Specific Electrical Resistance [µΩm], Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] in a range of (20;500)°C.